DTIC AD0819924: EFFECT OF SULFUR IN JP-5 FUEL ON HOT CORROSION OF COATED SUPERALLOYS IN MARINE ENVIRONMENT

Specimens of a nickel-base alloy (Mar M-200) with an aluminum- diffusion coating (Misco MDC-1) were tested using a high-pressure combustor facility to simulate environment in the turbine section of an aircraft engine….